Optical constants of Ir (Iridium)
Hass et al. 1967: n,k 0.005–0.546 µm; deposited at 300 °C

Wavelength: µm
 (0.0500 – 0.5461)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions & Spec sheet

n_absolute: true
wavelength_vacuum: false
substrate: glass
deposition_temperature: 300 °C

Comments

Thin film deposited at 300 °C

References

G. Hass, G. F. Jacobus, W. R. Hunter. Optical properties of evaporated iridium in the vacuum ultraviolet from 500 Å to 2000 Å, J. Opt. Soc. Am. 57, 758-762 (1967)