Optical constants of InSb (Indium antimonide)
Djurišić et al. 2000: n,k 0.207–0.827 µm
Wavelength:
µm
(2.0664e-01 – 1.2398e+00)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
References
A. B. Djurišić, E. H. Li, D. Rakić, M. L. Majewski. Modeling the optical properties of AlSb, GaSb, and InSb, Appl. Phys. A 70, 29-32 (2000)
[Calculation script (Python)]