Optical constants of He (Helium)
Smith et al. 1976: n 0.168–0.288 µm
Wavelength:
µm
(0.16796 – 0.28824)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true temperature: 0 °C pressure: 101325 Pa
Comments
Standard conditions: 0 °C (273.15 K), 760 torr (101.325 kPa).
References
P. L. Smith, M. C. E. Huber, W. H. Parkinson. Refractivities of H2, He, O2, CO, and Kr for 168≤λ≤288 nm Phys Rev. A 13, 199-203 (1976)