Optical constants of H2O, D2O (Water, heavy water, ice)
Warren and Brandt 2008: Ice; n,k 0.00443–2e6 µm
Wavelength:
µm
(4.430E-002 – 2.000E+006)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
temperature: -7 °C
Comments
Water ice (solid H2O) at -7 °C
References
S. G. Warren, and R. E. Brandt. Optical constants of ice from the ultraviolet to the microwave: A revised compilation, J. Geophys. Res. 113, D14220 (2008)
Optical constants available online at https://atmos.washington.edu/ice_optical_constants/