Optical constants of H2O, D2O (Water, heavy water, ice)
Warren 1984: Ice; n,k 0.00443–167 µm
Wavelength:
µm
(4.430E-2 – 1.670E+2)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
temperature: -7 ℃
Comments
Water ice (solid H2O) at -7 ℃
References
S. G. Warren. Optical constants of ice from the ultraviolet to the microwave, Appl. Opt. 23, 1206-1225 (1984)