Optical constants of H2O, D2O (Water, heavy water, ice)
Wang et al. 2016: Heavy water; k 1.2-2.6 µm
Wavelength:
µm
(1.200 – 2.600)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
temperature: 22 °C
Comments
22 °C.
References
Y. Wang, W. Wen, K. Wang, P. Zhai, P. Qiu, K. Wang. Measurement of absorption spectrum of deuterium oxide (D2O) and its application to signal enhancement in multiphoton microscopy at the 1700-nm window, Appl. Phys. Lett. 108, 021112 (2016)