Optical constants of H2O, D2O (Water, heavy water, ice)
Rowe et al. 2020: Water; n,k 0.667–10400 µm; -20 °C
Wavelength:
µm
(6.6668373E-01 – 1.0395939E+04)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true temperature: -20 °C
Comments
Supercooled liquid water (H2O) at -20 °C
References
P. M. Rowe, M. Fergoda, and S. Neshyba. Temperature-dependent optical properties of liquid water from 240 to 298 K, J. Geophys. Res. Atmos. 125, e2020JD032624 (2020) (Numerical data kindly provided by Penny Rowe)