Optical constants of H2O, D2O (Water, heavy water, ice)
Kofman et al. 2019: Amorphous ice; n 0.210-0.757 µm; 30 K
Wavelength:
µm
(0.21 – 0.757)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.374λ^2}{λ^2-0.071^2}+\frac{0.099λ^2}{λ^2-0.134^2}$$Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true temperature: 30 K
Comments
Amorphous water ice at 30 K.
References
V. Kofman, J. He, I. L. ten Kate, H. Linnartz. The refractive index of amorphous and crystalline water ice in the UV–vis, Astrophys. J. 875, 131 (2019)