Optical constants of Fe2O3 (Iron sesquioxide, Hematite)
Querry 1985: α-Fe2O3 (Hematite); n,k(e) 0.21–55.6 µm
Wavelength:
µm
(0.2100 – 55.5556)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
α-Fe2O3 (Hematite). Extraordinary ray (e).
References
M. R. Querry. Optical constants, Contractor Report CRDC-CR-85034 (1985)
Data
INFO
Iron sesquioxide, Fe2O3
Other names
- Iron(III) oxide
- Diiron trioxide
- Iron oxide
- Ferric oxide
- Ferric iron
- Red iron oxide
- Rouge
- Colcothar
- Rust
- Ochre
Minerals
- Hematite (haematite)
- Maghemite