Optical constants of Cs (Caesium)
Whang et al. 1971: n,k 0.129–0.344 µm
Wavelength:
µm
(0.1294 – 0.3444)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true
References
U. S. Whang, E. T. Arakawa, T. A. Callcott. Optical properties of Cs for photons of energy 3.6–9.6 eV, J. Opt. Soc. Am. 61, 740-745 (1971)
Data
INFO
Caesium (Cs)
Other name
- Cesium (American spelling)