Optical constants of CdGa2S4 (Cadmium gallium sulfide)
Kato et al. 2017: n(o) 0.490–7.52 µm
Wavelength:
µm
(0.49 – 7.519)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=6.49757+\frac{0.17227}{λ^2-0.02424}+\frac{315.22}{λ^2-328.19}$$Comments
Room temperature. Ordinary ray (o).
References
K. Kato, N. Umemura, V. Petrov. Sellmeier and thermo-optic dispersion formulas for CdGa2S4 and their application to the nonlinear optics of Hg1−xCdxGa2S4, Opt. Commun. 386, 49-52 (2017)
Data
INFO
Cadmium gallium sulfide, CdGa2S4
Other names
- Cadmium thiogallate
- Cadmium gallium sulphide