Optical constants of CS2 (Carbon disulfide)
Chemnitz et al. 2017: n 0.3-12 µm
Wavelength:
µm
(0.3 – 12)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.499426λ^2}{λ^2-0.178763^2}+\frac{0.089531λ^2}{λ^2-6.591946^2}$$Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true temperature: 20 °C
Comments
20 °C.
References
M. Chemnitz, M. Gebhardt, C. Gaida, F. Stutzki, J. Kobelke, J. Limpert, A. Tünnermann, M. A. Schmidt. Hybrid soliton dynamics in liquid-core fibres, Nat. Commun. 8, 42 (2017)