Optical constants of C (Carbon, diamond, graphite, graphene, carbon nanotubes)
Song et al. 2020: Carbon nanotubes film, HiPco grown; n,k 0.370–1.69 µm
Wavelength:
µm
(0.37096 – 1.68724)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true substrate: Si/SIO2
Comments
Carbon nanotubes. High-pressure carbon monoxide (HiPco) grown semiconducting single wall carbon nanotube (s-SWCNT) film on Si/SiO2 substrate.
References
B. Song, F. Liu, H. Wang, J. Miao, Y. Chen, P. Kumar, H. Zhang, X. Liu, H. Gu, E. A. Stach, X. Liang, S. Liu, Z. Fakhraai, D. Jariwala. Giant gate-tunability of complex refractive index in semiconducting carbon nanotubes, ACS Photonics 7, 2896-2905 (2020)
(see Supporting information for details)
Data
INFO
Carbon, C
Most common allotropes
- Diamond (cubic carbon)
- Graphite
- Amorphous carbon
- Graphene
- Carbon nanotube