Optical constants of C (Carbon, diamond, graphite, graphene, carbon nanotubes)
Querry 1985: Graphite pellet, Asbury Micro 260; n,k 0.21–55.6 µm
Wavelength:
µm
(0.2100 – 55.5556)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
Graphite pellet from Asbury Micro 260 powder.
References
M. R. Querry. Optical constants, Contractor Report CRDC-CR-85034 (1985)
Data
INFO
Carbon, C
Most common allotropes
- Diamond (cubic carbon)
- Graphite
- Amorphous carbon
- Graphene
- Carbon nanotube