Optical constants of C (Carbon, diamond, graphite, graphene, carbon nanotubes)
Ermolaev et al. 2020: Carbon nanotubes film, aerosol CVD; n,k 0.250-3.30 µm
Wavelength:
µm
(0.250 – 3.300)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true substrate: glass
Comments
Broadband optical constants of aerosol CVD SWCNTs in the spectral range 250–3300 nm.
References
G. A. Ermolaev, A. P. Tsapenko, V. S. Volkov, A. S. Anisimov, Y. G. Gladush, A. G. Nasibulin, Express determination of thickness and dielectric function of single-walled carbon nanotube films, Appl. Phys. Lett., 116, 231103 (2020) (Numerical data kindly provided by Georgy Ermolaev)
Data
INFO
Carbon, C
Most common allotropes
- Diamond (cubic carbon)
- Graphite
- Amorphous carbon
- Graphene
- Carbon nanotube