Optical constants of Bi2Se3 (Bismuth selenide)
Fang et al. 2020: 4-layer (4L) film; n,k 0.193-1.69 µm
Wavelength:
µm
(0.1930 – 1.6900)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true film_thickness: 4L substrate: sapphire
Comments
4-layer, 4L
References
M. Fang, Z. Wang, H. Gu, M. Tong, B. Song, X. Xie, T. Zhou, X. Chen, H. Jiang, T. Jiang, S. Liu, Layer-dependent dielectric permittivity of topological insulator Bi2Se3 thin films. Appl. Surf. Sci. 509, 144822 (2020) (Numerical data kindly provided by Baokun Song)
Data
INFO
Bismuth selenide, Bi2Se3
Other names
- Bismuth(III) selenide
- Dibismuth triselenide
- Selenoxobismuth
- Selanylidenebismuth