Optical constants of BaTiO3 (Barium titanate)
Wemple et al. 1968: n(e) 0.4–0.7 µm

Wavelength: µm
 (0.4 – 0.7)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{4.064λ^2}{λ^2-0.211^2}$$

Comments

Extraordinary ray (e). Room temperature

References

S.H. Wemple, M. Didomenico Jr., and I. Camlibel. Dielectric and optical properties of melt-grown BaTiO3, J. Phys. Chem. Solids 29, 1797-1803 (1968)