Optical constants of Au (Gold)
Yakubovsky et al. 2017: 117-nm film; n,k 0.3-2 µm
Wavelength:
µm
(0.3 – 2)
Derived optical constants
n
k
logX
logY
eV
Comments
Au thickness = 117 nm, e-beam evaporated at 1 Å/s with base pressure of 7e-7 Torr on Si wafer at T = 20 °C. Thickness determined by AFM and XRR.
References
D. I. Yakubovsky, A. V. Arsenin, Y. V. Stebunov, D. Yu. Fedyanin, V. S. Volkov. Optical constants and structural properties of thin gold films, Opt. Express 25, 25574-25587 (2017)