Optical constants of Au (Gold)
Magnozzi et al. 2019: n,k 0.252–1.45 µm; 225 °C

Wavelength: µm
 (0.25157–1.4492)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions & Spec sheet

n_is_absolute: true
wavelength_is_vacuum: true
temperature: 225 °C

Comments

Optically-thick and morphologically-flat Au film at 225 °C.

References

M. Magnozzi, M. Ferrera, L. Mattera, M. Canepa, F. Bisio. Plasmonics of Au nanoparticles in a hot thermodynamic bath, Nanoscale, 11, 1140–1146 (2019) (Numerical data kindly provided by Michele Magnozzi)