Optical constants of Au (Gold)
Lemarchand 2013: 4.62-nm film; n,k 0.35-1.8 µm
Wavelength:
µm
(0.350 – 1.800)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
4.62-nm monolayer deposited using the magnetron sputtering technique; thicknesses determined by X-ray diffraction.
References
F. Lemarchand, private communications (2013). Index determination is performed using method explained in:
L. Gao, F. Lemarchand, and M. Lequime. Comparison of different dispersion models for single layer optical thin film index determination, Thin Solid Films 520, 501-509 (2011)