Optical constants of Au (Gold)
Ciesielski et al. 2018: Au/SiO2; n,k 0.191–20.9 µm
Wavelength:
µm
(0.19077 – 20.912)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true film_thickness: 35 nm substrate: SiO2
Comments
35 nm-thick gold film deposited directly on SiO2 substrate
References
A. Ciesielski, L. Skowronski, M. Trzinski, E. Gorecka, P. Trautman, T. Szoplik. Evidence of germanium segregation in gold thin films, Surf. Sci. 674, 73-78 (2018) (Numerical data kindly provided by Arkadiusz Ciesielski)