Optical constants of As2Se3 (Arsenic triselenide)
Joseph et al. 2020: 700-nm film; n,k 0.246-1.69 µm
Wavelength:
µm
(0.2458 – 1.6880)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true film_thickness: 700 nm substrate: glass
Comments
700 nm film on glass substrate.
References
S. Joseph, S. Sarkar, J. Joseph, Grating-coupled surface plasmon-polariton sensing at a flat metal–analyte interface in a hybrid-configuration, ACS Appl. Mater. Interfaces, 12, 46519-46529 (2020)
(Numerical data kindly provided by Prof. Joby Joseph)
Data
INFO
Arsenic triselenide, As2Se3
Other names
- Arsenic(III) selenide
- Diarsenic triselenide
- Arsenic selenide