Optical constants of Al2O3 (Aluminium sesquioxide, Sapphire, Alumina)
Querry 1985: Thin film (oxidized Al mirror); n,k 0.21–12.5 µm
Wavelength:
µm
(0.2100 – 12.5000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Comments
Oxidized Al mirror.
References
M. R. Querry. Optical constants, Contractor Report CRDC-CR-85034 (1985)
Data
INFO
Aluminium sesquioxide, Al2O3
Other names
- Alumina
- Aluminium oxide
- Aloxite
- Aluminium oxide (α)
- Aluminium(III) oxide
- Dialuminium trioxide
Mineral
- Corundum
Gemstones
- Sapphire
- Ruby