Optical constants of Al (Aluminium)
Rakić et al. 1998: Brendel-Bormann model; n,k 0.0620-248 µm
Wavelength:
µm
(6.1992e-02 – 2.4797e+02)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true
Comments
Fit of experimental data from several sources to Brendel-Bormann (BB) model
References
A. D. Rakić, A. B. Djurišic, J. M. Elazar, and M. L. Majewski. Optical properties of metallic films for vertical-cavity optoelectronic devices, Appl. Opt. 37, 5271-5283 (1998)
[Calculation script (Python)]