Optical constants of AgGaSe2 (Silver gallium selenide, AGSe)
Kato et al. 2021: n(o) 0.81–18 µm
Wavelength:
µm
(0.81 – 18)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=11.62264+\frac{0.43221}{λ^2-0.15597}+\frac{18868.52}{λ^2-3953.34}$$Comments
Ordinary ray (o) 20–22 °C.
References
K. Kato, K. Miyata, V. Petrov. Refined Sellmeier equations for AgGaSe2 up to 18 µm, Appl. Opt., 60, 805–808 (2021)