Optical constants of Ag (Silver)
Werner et al. 2009: DFT calculations; n,k 0.0176–2.48 µm
Wavelength:
µm
(0.017586 – 2.479684)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true
Comments
Theoretical density function theory (DFT) calculations.
References
W. S. M. Werner, K. Glantschnig, C. Ambrosch-Draxl. Optical constants and inelastic electron-scattering data for 17 elemental metals, J. Phys Chem Ref. Data 38, 1013-1092 (2009)