RefractiveIndex.INFO

Refractive index database


Shelf

Book

Page

Optix.eXpert is our new website that aims at connecting optical professionals with employers looking to outsource optics related work. Sign up and fill out a short form to start offering your service!

Optical constants of Ag (Silver)
Johnson and Christy 1972: n,k 0.188-1.94 µm

Wavelength: µm
 (0.1879 – 1.9370)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Comments

Room temperature

References

P. B. Johnson and R. W. Christy. Optical constants of the noble metals, Phys. Rev. B 6, 4370-4379 (1972)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Silver, Ag

Silver is often used as a coating material for broadband mirrors for visible and infrared spectral regions.

External links