Optical constants of Ag (Silver)
Ferrera et al. 2019: n,k 0.245–1.45 µm; 600 K
Wavelength:
µm
(0.245202–1.449249)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_is_absolute: true wavelength_is_vacuum: true temperature: 600 K substrate: Si/SiO2
Comments
600 K (327 °C). Optically thick and morphologically flat polycrystalline Ag film, deposited by molecular beam epitaxy on a silicon wafer with a native oxide substrate.
The supplemental material of the original publication provides extra information by including additional data for 25 temperatures within the range of 298–600 K.
References
M. Ferrera, M. Magnozzi, F. Bisio, M. Canepa. Temperature-dependent permittivity of silver and implications for thermoplasmonics, Phys. Rev. Mater., 3, 105201 (2019) (See Supplemental Material for numerical data)