Optical constants of Ag (Silver)
Ciesielski et al. 2017: Ag/Ge/SiO2; n,k 0.191-20.9 µm
Wavelength:
µm
(0.19077 – 20.912)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true film_thickness: 20 nm substrate: Ge/SiO2
Comments
20 nm-thick silver film deposited on SiO2 substrate with 2 nm-thick Ge wetting interlayer
References
A. Ciesielski, L. Skowronski, M. Trzinski, T. Szoplik. Controlling the optical parameters of self-assembled silver films with wetting layers and annealing, Appl. Surf. Sci. 421B, 349-356 (2017) (Numerical data kindly provided by Arkadiusz Ciesielski)