Optical constants of Ag (Silver)
Choi et al. 2020: n,k 1.23–6.99 µm
Wavelength:
µm
(1.231 – 6.988)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions & Spec sheet
n_absolute: true wavelength_vacuum: true
Comments
Epitaxially grown, atomically smooth, single crystalline thick Ag film. Room temperature.
References
J. Choi, F. Cheng, J. W. Cleary, L. Sun, C. K. Dass, J. R. Hendrickson, C.-Y. Wang, S. Gwo, C.-K. Shih, X. Li. Optical dielectric constants of single crystalline silver films in the long wavelength range, Opt. Mater. Express 10, 693-703 (2020)
(see supplementary materials for numerical data)