Optical constants of Soda lime glass
Rubin 1985: Bronze; n,k 0.32–4.6 µm

Wavelength: µm
 (0.32–4.6)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.5130-0.003169λ^{2}+0.003962λ^{-2}$$

Comments

Bronze soda lime silica window glass

References

M. Rubin. Optical properties of soda lime silica glasses, Sol. Energy Mater. 12, 275-288 (1985)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Soda lime glass

Soda-lime glass is the most prevalent type of glass, used for windowpanes and glass containers. Soda-lime glass accounts for about 90% of manufactured glass.