Optical constants of Soda lime glass
Rubin 1985: Far-infared; n,k 5–300 µm

Wavelength: µm
 (5.0 – 300.0)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Comments

Soda lime silica window glass in the far-infrared. Opticsl constants are same for clear, colored (bronze, grey, green) and low-iron glass.

References

M. Rubin. Optical properties of soda lime silica glasses, Sol. Energy Mater. 12, 275-288 (1985)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Soda lime glass

Soda-lime glass is the most prevalent type of glass, used for windowpanes and glass containers. Soda-lime glass accounts for about 90% of manufactured glass.