Optical constants of SUMITA - ZnSF
K-ZnSF8(M)
Wavelength:
µm
(0.340 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.8508369-0.012006057λ^{2}+0.025904826λ^{-2}+0.0009056149λ^{-4}-2.8090015\text{×}10^{-05}λ^{-6}+4.695922\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 1.49e-05 1.99e-08 -2.6e-10 8.88e-07 7.78e-10 0.234 nd: 1.71143 Vd: 38.9 glass_code: 714389 density: 3.72 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 4.9e-06 K-1 - temperature_range: 20 300 °C coefficient: 6e-06 K-1 dPgF: -0.0047 climatic_resistance: 2.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book