Optical constants of SUMITA - VC
K-VC99
Wavelength:
µm
(0.310 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.3294765-0.015324675λ^{2}+0.031941277λ^{-2}+0.0010078745λ^{-4}-2.8400554\text{×}10^{-05}λ^{-6}+3.488686\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 4.51e-06 1.51e-08 -2.57e-10 7.41e-07 8.37e-10 0.205 nd: 1.85060 Vd: 41.6 glass_code: 851416 density: 5.15 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.3e-06 K-1 dPgF: -0.0102 climatic_resistance: 1.0 acid_resistance: 2.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book