Optical constants of SUMITA - VC
K-VC90(M)
Wavelength:
µm
(0.330 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.3149515-0.013619007λ^{2}+0.033842693λ^{-2}+0.001108869λ^{-4}-2.8110622\text{×}10^{-05}λ^{-6}+5.1120171\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 4.39e-07 1.31e-08 -1.78e-10 7.82e-07 9.78e-10 0.232 nd: 1.84859 Vd: 38.9 glass_code: 853390 density: 4.98 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.7e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.4e-06 K-1 dPgF: -0.0057 climatic_resistance: 1.0 acid_resistance: 2.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book