Optical constants of SUMITA - VC
K-VC82(M)
Wavelength:
µm
(0.320 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.9914895-0.01436707λ^{2}+0.024650584λ^{-2}+0.00071568019λ^{-4}-2.7938999\text{×}10^{-05}λ^{-6}+3.2293973\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 5.27e-06 1.73e-08 -7.19e-11 6.68e-07 9.93e-10 0.203 nd: 1.75028 Vd: 45.4 glass_code: 756456 density: 4.25 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.9e-06 K-1 - temperature_range: 20 300 °C coefficient: 8e-06 K-1 dPgF: -0.0098 climatic_resistance: 1.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book