Optical constants of SUMITA - VC
K-VC79
Wavelength:
µm
(0.270 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5520489-0.011234947λ^{2}+0.014455084λ^{-2}+0.00046725318λ^{-4}-3.6714004\text{×}10^{-05}λ^{-6}+2.2810504\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 5.06e-07 1.46e-08 -2.13e-11 4.85e-07 4.45e-11 0.187 nd: 1.61035 Vd: 57.9 glass_code: 610579 density: 3.09 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.2e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.3e-06 K-1 dPgF: -0.0058 climatic_resistance: 2.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book