Optical constants of SUMITA - VC
K-VC185(M)
Wavelength:
µm
(0.320 – 2.000)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=3.3218568-0.014962898λ^{2}+0.032206874λ^{-2}+0.0011931823λ^{-4}-5.072415\text{×}10^{-05}λ^{-6}+5.1953408\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 4.01e-06 1.77e-08 -2.37e-10 7.39e-07 1.02e-09 0.227 nd: 1.84909 Vd: 40.5 glass_code: 854406 density: 5.0 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.8e-06 K-1 - temperature_range: 20 300 °C coefficient: 7e-06 K-1 dPgF: -0.009 climatic_resistance: 1.0 acid_resistance: 3.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book