Optical constants of SUMITA - VC
K-VC181(M)
Wavelength:
µm
(0.340 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.1735917-0.01381902λ^{2}+0.029219972λ^{-2}+0.0011233335λ^{-4}-4.4143284\text{×}10^{-05}λ^{-6}+4.6335289\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 6.99e-06 2.24e-08 -2.94e-10 8.37e-07 3.41e-10 0.213 nd: 1.80614 Vd: 41.1 glass_code: 811411 density: 4.71 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.7e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.9e-06 K-1 dPgF: -0.0061 climatic_resistance: 1.0 acid_resistance: 3.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book