Optical constants of SUMITA - VC
K-VC179(M)
Wavelength:
µm
(0.340 – 2.000)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=3.1342666-0.013761215λ^{2}+0.028817199λ^{-2}+0.00082006501λ^{-4}-5.3846865\text{×}10^{-06}λ^{-6}+2.2272066\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 5.81e-06 1.54e-08 -1.28e-10 7.89e-07 6.03e-10 0.215 nd: 1.79441 Vd: 41.9 glass_code: 799418 density: 4.65 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.1e-06 K-1 - temperature_range: 20 300 °C coefficient: 8e-06 K-1 dPgF: -0.0058 climatic_resistance: 1.0 acid_resistance: 3.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book