Optical constants of SUMITA - VC
K-VC100(M)
Wavelength:
µm
(0.330 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.1544352-0.014806744λ^{2}+0.027996766λ^{-2}+0.00079379644λ^{-4}-1.0802615\text{×}10^{-05}λ^{-6}+2.172329\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 4.79e-06 1.51e-08 -1.35e-10 6.25e-07 7.77e-10 0.229 nd: 1.79916 Vd: 43.5 glass_code: 804436 density: 4.71 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.8e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.2e-06 K-1 dPgF: -0.008 climatic_resistance: 1.0 acid_resistance: 3.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book