Optical constants of SUMITA - SSK (Very dense flint)
K-SSK3
Wavelength:
µm
(0.290 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5591851-0.0099057522λ^{2}+0.016577727λ^{-2}+0.00054738619λ^{-4}-3.5329686\text{×}10^{-05}λ^{-6}+2.4596919\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 8.96e-06 1.89e-08 -2.12e-10 6.71e-07 9.18e-10 0.191 nd: 1.61484 Vd: 51.1 glass_code: 615511 density: 3.37 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.6e-06 K-1 - temperature_range: 20 300 °C coefficient: 7.2e-06 K-1 dPgF: -0.0072 climatic_resistance: 1.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book