Optical constants of SUMITA - SKF
K-SKF6
Wavelength:
µm
(0.320 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.2505164-0.0088684142λ^{2}+0.012260534λ^{-2}+0.00042234633λ^{-4}-2.1095054\text{×}10^{-05}λ^{-6}+2.2440064\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -9.67e-06 1.6e-08 -1.08e-10 4.97e-07 6.44e-11 0.231 nd: 1.51200 Vd: 52.1 glass_code: 512521 density: 2.51 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 9.5e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 1e-05 K-1 dPgF: 0.0035 climatic_resistance: 1.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book