Optical constants of SUMITA - SK (Dense crown)
K-SK15
Wavelength:
µm
(0.290 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.5918508-0.010567563λ^{2}+0.014411695λ^{-2}+0.00063226961λ^{-4}-5.7927037\text{×}10^{-05}λ^{-6}+3.4193172\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -1.08e-06 1.69e-08 -2.15e-10 4.4e-07 6.37e-10 0.19 nd: 1.62299 Vd: 58.1 glass_code: 623581 density: 3.67 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.8e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 8e-06 K-1 dPgF: -0.0023 climatic_resistance: 3.0 acid_resistance: 4.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book