Optical constants of SUMITA - SK (Dense crown)
K-SK14

Wavelength: µm
 (0.280 – 2.000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=2.5313894-0.010956275λ^{2}+0.013803544λ^{-2}+0.00029803889λ^{-4}-6.2451964\text{×}10^{-06}λ^{-6}+2.5686024\text{×}10^{-07}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 °C
thermal_dispersion:
  - type: "Schott formula"
    coefficients: 5.63e-07 2.16e-08 -8.94e-11 4.28e-07 2.18e-10 0.16
nd: 1.60311
Vd: 60.7
glass_code: 603607
density: 3.44 g/cm3
thermal_expansion:
  - temperature_range: -30 70 °C
    coefficient: 5.7e-06 K-1
  - temperature_range: 20 300 °C
    coefficient: 7.3e-06 K-1
dPgF: -0.0011
climatic_resistance: 3.0
acid_resistance: 4.0

References

SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

SUMITA Optical Glass, Inc.

SUMITA Optical Glass, Inc. is a Japanese glass manufacturer