Optical constants of SUMITA - SFLD
K-SFLD8
Wavelength:
µm
(0.360 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.7609221-0.011601354λ^{2}+0.029309701λ^{-2}+0.0012957192λ^{-4}-3.6971081\text{×}10^{-05}λ^{-6}+9.8723481\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -9.37e-07 1.62e-08 -1.83e-10 7.05e-07 1.05e-09 0.299 nd: 1.68893 Vd: 31.1 glass_code: 689311 density: 2.94 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.7e-06 K-1 dPgF: 0.0062 climatic_resistance: 1.0 acid_resistance: 1.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book