Optical constants of SUMITA - SFLD
K-SFLD6
Wavelength:
µm
(0.370 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.1176009-0.012108189λ^{2}+0.044689743λ^{-2}+0.0016574765λ^{-4}+4.1984442\text{×}10^{-05}λ^{-6}+1.29135\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -6.59e-06 1.77e-08 -2.13e-10 1.11e-06 8.72e-10 0.277 nd: 1.80518 Vd: 25.4 glass_code: 805254 density: 3.4 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9.3e-06 K-1 - temperature_range: 20 300 °C coefficient: 1.07e-05 K-1 dPgF: 0.0136 climatic_resistance: 1.0 acid_resistance: 1.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book