$$n^2=2.9621759-0.011836005λ^{2}+0.037648353λ^{-2}+0.0015341601λ^{-4}-1.0776303\text{×}10^{-05}λ^{-6}+1.378924\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -2.91e-06 1.97e-08 -3.23e-10 8.95e-07 9.72e-10 0.291 nd: 1.75520 Vd: 27.5 glass_code: 755275 density: 3.19 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 8.6e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.1e-06 K-1 dPgF: 0.0131 climatic_resistance: 1.0 acid_resistance: 1.0