Optical constants of SUMITA - SFLD
K-SFLD1

Wavelength: µm
 (0.360 – 2.000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=2.8465679-0.01179579λ^{2}+0.032766631λ^{-2}+0.0014514223λ^{-4}-4.8225155\text{×}10^{-05}λ^{-6}+1.2981324\text{×}10^{-05}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 20.0 °C
thermal_dispersion:
  - type: "Schott formula"
    coefficients: -2e-06 1.26e-08 -4.49e-10 9.35e-07 1.09e-09 0.27
nd: 1.71736
Vd: 29.5
glass_code: 717295
density: 3.03 g/cm3
thermal_expansion:
  - temperature_range: -30 70 °C
    coefficient: 8.2e-06 K-1
  - temperature_range: 20 300 °C
    coefficient: 9.7e-06 K-1
dPgF: 0.0075
climatic_resistance: 1.0
acid_resistance: 1.0

References

SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

SUMITA Optical Glass, Inc.

SUMITA Optical Glass, Inc. is a Japanese glass manufacturer

External links


Glass

External links