Optical constants of SUMITA - PSK (Dense phosphate crown)
K-PSKn2
Wavelength:
µm
(0.310 – 2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.578886-0.010381408λ^{2}+0.014233563λ^{-2}+0.00012483021λ^{-4}+1.7477672\text{×}10^{-05}λ^{-6}-9.6204805\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -9.04e-06 1.1e-08 -2.48e-10 3.21e-07 4.56e-10 0.226 nd: 1.61800 Vd: 63.4 glass_code: 618634 density: 3.63 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.9e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.9e-06 K-1 dPgF: 0.0055 climatic_resistance: 1.0 acid_resistance: 5.0
References
SUMITA Zemax catalog 2017-02-02 (obtained from http://www.sumita-opt.co.jp)
See also SUMITA optical glass data book